Recycled Ceramic Permeable Pavers
Made with aggregate processed from waste ceramics, for permeable paving that supports the urban water cycle.

GALLERY






PERFORMANCE
Performance
4.4 MPa
Flexural strength
Tested by KTR
1.12 mm/s
Permeability coefficient
Tested by KTR
Grade 2
Permeability retention
Tested by KTR
KTR testing confirmed a flexural strength of 4.4 MPa, a permeability coefficient of 1.12 mm/s and Grade 2 permeability retention. Long-term performance is still being monitored.



KTR Certified Test Report
Issued by the Korea Testing & Research Institute (KTR). The original PDFs (Korean and English) are not available for download; we will send them to you directly on request.
Available on requestPROCESS
From waste ceramics to a paving block

01
Waste ceramics
We source and sort usable raw materials.

02
Processed aggregate
We crush the ceramics and control the particle size.

03
Mixing & molding
We mix the material and press it into blocks.

04
Installation
Installed on site the same way as conventional permeable paving blocks.

SPECIFICATION
Specifications
- Product type
- Permeable paving block made with waste ceramic aggregate
- Dimensions
- 200 × 200 × 60 mm
- Colors
- White · Gray
- Main material
- Processed waste ceramic aggregate
- Applications
- Walkways · Public sidewalks · Building exteriors
- Installation
- Installed the same way as conventional permeable paving blocks

White

Gray
Available in two colors: white and gray
Need product documents?
Product documents are available in Resources; test reports are sent on request.